Line 130: Line 130:
   - Use ethanol and paper tissue to remove the remaining photoresist from the board(s). Be thorough.   - Use ethanol and paper tissue to remove the remaining photoresist from the board(s). Be thorough.
   - Let the board(s) dry. You can also use compressed air to speed things up.   - Let the board(s) dry. You can also use compressed air to speed things up.
 +  - If you do not plan on soldering the PCBs on the same day, use solderable protective resin ("Lötlack") to protect the copper from oxidizing.
   - Clean the lab equipment, rinse everything with water.   - Clean the lab equipment, rinse everything with water.
   - Dispose of waste properly.    - Dispose of waste properly. 