| - dry the board using paper towels | - dry the board using paper towels | ||
| - Use alcohol wipes to remove the remaining photo-resist from the board. Be thorough, this will show up as blackness on wipe. | - Use alcohol wipes to remove the remaining photo-resist from the board. Be thorough, this will show up as blackness on wipe. | ||
| - | - If you do not plan on soldering the PCBs on the same day, use solderable protective resin ("Lötlack") to protect the copper from oxidizing. | + | - If you do not plan on soldering the PCBs on the same day, use solderable protective resin ("Lötlack") to protect the copper from oxidizing. |
| - Dispose of waste properly. | - Dispose of waste properly. | ||